E max ceram porcelain build up.
Ips e max zirpress is a combination of lithium disilicate and zirconium dioxide wherein lithium disilicate is pressed on to zirconium dioxide for enhancing its properties.
Choose the suitable framework material in accordance with the indication and the required strength.
Ips e max ceram is the highly esthetic layering ceramic for the ips e max system.
Ips e max zircad block partially sintered zirconium oxide stabilized with yttrium oxide was the core material while a2 ht and lt ips e max zirpress fluorapatite glass ceramic ingot for heat pressing a2 ips e max ceram low fusing nano fluorapatite dentin porcelain for.
96 0 e max system 96 0 e max press 96 0 e max cad 94 9 e max ceram 96 0 e max zircad ips e max is a material that satisfies my esthetic needs in the anterior and my functional needs in the posterior david hornbrook dds.
Powders mixed with the soft liquid demonstrate a shorter processing time.
Ips e max ceram is suitable for efficient standard layering as well as for demanding high end layering with lifelike play of light.
Lithium disilicate glass ceramic ls 2 or zirconium oxide zro 2 your dental technician can veneer all the ips e max materials with ips e max ceram.
The material forms part of the ips e max system and is designed for the veneering of frameworks made of ips e max lithium disilicate glass ceramics ls 2 and zirconium oxide zro 2.
The classic dentin and incisal materials are ideally coordinated with more opaque all ceramic framework structures and thus are ideally suitable for the veneering of more opaque substructures.
Ips e max ceram is a highly esthetic fluorapatite layering ceramic that offers a proven track record of over ten years.
Ips e max all ceramic system ivoclar vivadent schaan liechtenstein was selected to fabricate the specimens.
If build up liquids other than the ips e max ceram liquids are used therefore there is a risk of incomplete burn out and thus discolouration of the restorati on e g.
The good news is even with a thickness of 1 mm emax crowns carry a flexural strength of 500 mpa.